[1]郭 瑞,薛 河,崔英浩.安全端焊接残余应力对裂纹尖端力学参量的影响[J].西安科技大学学报,2018,(03):479-483.[doi:10.13800/j.cnki.xakjdxxb.2018.0319]
 GUO Rui,XUE He,CUI Ying-hao.Influence of residual stress in safety end on mechanical parameters at crack tip[J].Journal of Xi'an University of Science and Technology,2018,(03):479-483.[doi:10.13800/j.cnki.xakjdxxb.2018.0319]
点击复制

安全端焊接残余应力对裂纹尖端力学参量的影响(/HTML)
分享到:

西安科技大学学报[ISSN:1672-9315/CN:61-1434/N]

卷:
期数:
2018年03期
页码:
479-483
栏目:
出版日期:
2018-05-15

文章信息/Info

Title:
Influence of residual stress in safety end on mechanical parameters at crack tip
文章编号:
1672-9315(2018)03-0479-05
作者:
郭 瑞12薛 河1崔英浩1
1.西安科技大学 机械工程学院,陕西 西安 710054; 2.布鲁内尔大学 工程设计与自然科学学院,英国 伦敦 UB8 3PH
Author(s):
GUO Rui12XUE He1CUI Ying-hao1
(1.College of Mechanical and Engineering,Xi'an University of Science and Technology,Xi'an 710054,China; 2.College of Engineering,Design and Physical Sciences,Brunel University,London,UB8 3PH,United Kingdom)
关键词:
机械工程 结构完整性 数值模拟试验 应力腐蚀开裂 焊接残余应力
Keywords:
mechanical engineering structural integrity analysis welding residual stress material heterogeneity stress and strain
分类号:
O 346.1
DOI:
10.13800/j.cnki.xakjdxxb.2018.0319
文献标志码:
A
摘要:
焊接残余应力是导致核电一回路安全端异种金属焊接接头引导力腐蚀开裂(SCC)的主要因素之一,同时焊接接头区域材料力学性能不均匀性使得SCC裂纹尖端力学场分析变得更为复杂。为了了解核电一回路压力容器安全端异种焊接结构中残余应力对裂纹尖端力学参量的影响,本文通过有限元手段分别利用预定义温度场法和导入预应力法对核电一回路安全端焊接接头中的残余应力分布进行模拟,并计算分析了焊接残余应力作用对安全端焊接接头中SCC裂纹尖端主要力学参量的影响。研究表明,导入预应力法是较理想的焊接接头残余应力场模拟方法; 裂尖应力、应变以及J积分均与残余应力的分布规律有很大的关联性; 当裂纹长度小于管壁厚度的三分之一时,裂尖应力应变和断裂参量随裂纹长度增加而增大,之后趋于平稳; 当裂纹长度接近30 mm时裂尖法向应力由正变负,裂尖应力应变随裂纹长度的增大而减小,有可能造成SCC裂纹扩展停滞。研究结果为日后定量预测安全端SCC裂纹扩展历程奠定了一定的理论基础。
Abstract:
The welding residual stress is one of the main factors that lead to the Stress Corrosion Cracking(SCC)in dissimilar metal welded joints in the safety end of nuclear power plants.Additionally,the mechanical properties of the SCC crack tip become more complicated due to the heterogeneity of the mechanical properties of the welded joint.To understand the influence of residual stress on the crack tip mechanical parameters in the dissimilar welded structure of the safety end of a nuclear power circuit pressure vessel,the predefined temperature field method and the stress field introduction method were respectively used in Finite Element software.The residual stress distribution was simulated,and the effects of welding residual stress on the key mechanical parameters of the SCC crack tip in the welded joint were calculated and analyzed.The results show that the stress field introduction method is relatively an ideal method for the simulation of the residual stress field in welded joints.The stress,strain and J-integral around crack tips all have a significant correlation with the distribution of residual stress.When the crack length is less than one-third of the thickness of the pipe wall,the stress,strain and fracture parameters around crack tips increased while the crack length grew,but tend to be stable at the end.When the crack length is close to 30mm,the normal stress of the crack tip changes from positive to negative,and the crack tip stress and strain decreased then the crack length increased,which may cause SCC crack propagation stagnated.Our research provides a theoretical basis for the quantitative prediction of the SCC crack propagation history of the safety end in the future.

参考文献/References:

[1] 杨 武.核电工程材料的应力腐蚀破裂研究[J].腐蚀科学与防护技术,1995,7(2):87-92. YANG Wu.Stress corrosion cracking of engineering materials used in nuclear power plants[J].Corrosion Science and Protection Technique,1995,7(2):87-92.
[2] 杨 武.材料科技工作者面临我国核电大发展的机遇与挑战[J].腐蚀与防护,2005,26(4):182-183. YANG Wu.Material science and technology workers faced the opportunity and challenge of the development of nuclear power in China[J].Corrosion and Protection,2005,26(4):182-183.
[3] 韩恩厚.核电站关键材料在微纳米尺度上的环境损伤行为研究——进展与趋势[J].金属学报,2011,47(7):769-776. HAN En-hou.Research trends on micro and nano-scale materials degradation in nuclear power plant[J].Acta Metallurgica Sinica,2011,47(7):769-776.
[4]李光福.压水堆压力容器接管-主管安全端焊接件在高温水中失效案例和相关研究[J].核技术,2013,36(4):229-234. LI Guang-fu.Failure cases of welds between pressure vessel nozzle and main pipe safe-end in high temperature water environments and relevant research[J].Nuclear Techniques,2013,36(4):229-234.
[5]李光福,李冠军,方可伟,等.异材焊接件A508/52M/316L在高温水环境中的应力腐蚀破裂[J].金属学报,2011,47(7):797-803. LI Guang-fu,LI Guan-jun,FANG Ke-wei,et al.Stress corrosion cracking behavior of dissimilar metal weld A5008/52M/316L in high temperature water environment[J].Acta Metallugica Sinica,2011,47(7):797-803.
[6]董月香.几种应力腐蚀试验方法的比较[J].大型铸锻件,2010(5):45-47. DONG Yue-xiang.The comparison of stress corrosion test methods[J].Heavy Casting and Forging,2010(5):45-47.
[7]Xue H,Sato Y,Shoji T.Quantitative estimation of the growth of environmentally assisted cracks at flaws in light water reactor components[J].Journal of Pressure Vessel Technology,2009,131(1):11404-1-11404-9.
[8]Zinkle S J,Was G S.Materials challenges in nuclear energy[J].Acta Materialia,2013,61(3):735-758.
[9]赵 红,祝美丽.火电站新型中厚板异种钢焊接接头残余应力场数值模拟研究[J].热加工工艺,2006,35(19):77-79. ZHAO Hong,ZHU Mei-li.Stimulation study on residual stress field of welded joints of new grade dissimilar steel with middle thickness in power station[J].Hot Working Technology,2006,35(19):77-79.
[10]Hanninen H,Cullen W,Kemppainen M.Effects of MnS inclusion dissolution on environmentally assisted cracking in low-alloy and carbon steels[J].Corrosion,1990,46(7):563-573.
[11]Wells D B,Stewart J,Davidson R,et al.The mechanism of intergranular stress corrosion cracking of sensitised austenitic stainless steel in dilute thiosulphate solution[J].Corrosion science,1992,33(1):39-71.
[12]罗利伟,付小超.焊接残余应力的产生及其消除方法[J],山西建筑,2008,34(20):134-135. LUO Li-wei,FU Xiao-chao.Generation and erase method of residual stress by welding[J].Shanxi Architecture,2008,34(20):134-135.
[13]龚晓燕,焦 康,赵凌燕,等.焊接接头力学性能不均匀性对管道裂纹断裂参量的影响分析[J].西安科技大学学报,2013,33(2):211-215. GONG Xiao-yan,JIAO Kang,ZHAO Ling-yan,et al.Effect of welded mechanical heterogeneity on fracture parameters of pipeline cracks[J].Journal of Xi'an University of Science and Technology,2013,33(2):211-215.
[14]Lundin C D.Dissimilar metal welds-transition joints literature review[J].Welding Journal,1982,61(2):58-63.
[15]Hearn E J.Contact stress,residual stress and stress concentrations[J].Mechanics of materials,1997(2):381-442.
[16]Ren Y,Paradowska A,Wang B,et al.Residual stress state of X65 pipeline girth welds before and after local and furnace post weld heat treatment[J].Journal of Pressure Vessel Technology,2017,139(4):41401-1-41401-9.
[17]Zhao L,Xue H,Tang W,et al.Effect of welded mechanical heterogeneity on local stress and strain ahead of growing crack tips in the piping welds[C]//ASME 2011 Pressure Vessels and Piping Conference.American Society of Mechanical Engineers,2011:223-232.
[18]侯 娟,彭群家,庄子哲雄,等.镍基合金焊接过渡区微观结构及应力腐蚀行为研究[J].金属学报,2010,46(10):1258-1266. HOU Juan,PENG Qun-jia,Shoji T,et al.Study of microstructure and stress corrosion cracking behavior in welding transition zone of Ni-Base Alloys[J].Acta Metallurgica Sinica,2010,46(10):1258-1266.
[19]刘金依,薛 河,刘永军,等.三维中心裂纹板中J积分的计算及分析[J].西安科技学院学报,2002,22(1):91-94. LIU Jin-yi,XUE He,LIU Yong-jun,et al.Calculating and analyzing of J-integral in the center-cracked panel[J].Journal of Xi'an University of Science and Technology,2002,22(1):91-94.

相似文献/References:

[1]杨宏亮,薛 河,倪陈强.冷加工对316L不锈钢裂尖力学特性的影响[J].西安科技大学学报,2018,(03):484.[doi:10.13800/j.cnki.xakjdxxb.2018.0320]
 YANG Hong-liang,XUE He,NI Chen-qiang.Effect of cold working on mechanical properties at crack tip of 316L stainless steel[J].Journal of Xi'an University of Science and Technology,2018,(03):484.[doi:10.13800/j.cnki.xakjdxxb.2018.0320]
[2]杨 林,马宏伟,王川伟,等.校园巡检机器人智能导航与控制[J].西安科技大学学报,2018,(06):1013.[doi:10.13800/j.cnki.xakjdxxb.2018.0619]
 YANG Lin,MA Hong-wei,WANG Chuan-wei,et al.Intelligent navigation and control of campus inspection robot[J].Journal of Xi'an University of Science and Technology,2018,(03):1013.[doi:10.13800/j.cnki.xakjdxxb.2018.0619]
[3]高 扬,李佳璞,杨来侠,等.可降解药物控释系统的药物扩散系数表征[J].西安科技大学学报,2018,(06):1021.[doi:10.13800/j.cnki.xakjdxxb.2018.0620]
 GAO Yang,LI Jia-pu,YANG Lai-xia,et al.Diffusion coefficient expression of degradable controlled drug delivery system[J].Journal of Xi'an University of Science and Technology,2018,(03):1021.[doi:10.13800/j.cnki.xakjdxxb.2018.0620]
[4]张 宁,张幼振,陈 盼.煤矿巷道底鼓治理机群施工建模及优化配置[J].西安科技大学学报,2019,(01):96.[doi:10.13800/j.cnki.xakjdxxb.2019.0114 ]
 ZHANG Ning,ZHANG You-zhen,CHEN Pan.Construction modeling and optimal allocation of roadway floorheave control group in coal mine[J].Journal of Xi'an University of Science and Technology,2019,(03):96.[doi:10.13800/j.cnki.xakjdxxb.2019.0114 ]
[5]倪陈强,薛 河,赵凌燕,等.弧形双悬臂梁试样裂纹扩展电测接线点布局研究[J].西安科技大学学报,2019,(02):309.[doi:10.13800/j.cnki.xakjdxxb.2019.0218 ]
 NI Chen-qiang,XUE He,ZHAO Ling-yan,et al.Wire connection points layout of crack extension electrical measurement of contoured double cantilever beam specimen[J].Journal of Xi'an University of Science and Technology,2019,(03):309.[doi:10.13800/j.cnki.xakjdxxb.2019.0218 ]

备注/Memo

备注/Memo:
收稿日期:2017-08-15 责任编辑:李克永
基金项目:国家自然科学基金(51475362); 国家教育部博士点基金(20136121110001)
通信作者:薛 河(1961-),男,江苏扬州人,教授,博士生导师,E-mail:XUEHE1961@163.com
更新日期/Last Update: 2018-06-30